Brand Name: | JINXING |
---|---|
Model Number: | Inconel X750 Spring Wire |
Certification: | ISO 9001 |
Place of Origin: | China |
Minimum Order: | 5kg |
Price: | 10~200USD/kg |
Payment Terms: | L/C, D/A, D/P, T/T, Western Union |
Supply Ability: | 5tons/M |
Delivery Time: | 25~35days |
Packaging Details: | Plywood Case |
Material: | Inconel X750 UNS N07750 |
Surface: | Black or Polished |
Other named: | NiCr15Fe7TiAl, NC15FeTNbA, NCF750,GH4145 |
Heat Treatment: | Solution Annealing |
Density: | 8.25g/cm3 |
Melt Range: | 1395~1425℃ |